Edge rounding and slag removal before coating on structural steel

A GDM-265D removes dross from both faces of plasma-cut parts and a GCM-R3AR rounds the edges to R2 so the coating holds.

Edge rounding and slag removal before coating on structural steel

The Challenge

Coating systems for bridges and corrosive environments require rounded edges, and paint applied over cut-edge dross or sharp arrises thins out and fails first. Hand grinding hundreds of parts per shift is slow, inconsistent and hard on operators.

Our Solution

Parts leave the plasma table and pass through a GDM-265D, which strips dross and burrs from both faces, including around holes. Long edges are then rounded to R2 or R3 on a GCM-R3AR in one pass for both corners; small parts go over a table-type TCM-SR3-SP.

Workflow

  1. Plasma or flame cutting
  2. Deslag and deburr both faces on the GDM-265D
  3. Round edges to R2/R3 on the GCM-R3AR or TCM-SR3-SP
  4. Blast cleaning
  5. Coating

Result

Consistent edge radius on every part and clean surfaces into the blast room, replacing manual grinding at this stage.

EQUIPMENT

Machines Used in This Project

CONTACT US

Planning a Similar Project?

Tell us your material, plate thickness or pipe size and the bevel you need. Our engineers will recommend the right machine and send a quotation within 24 hours.

Send Us a Message

Fields marked * are required.

We reply within 24 hours on working days